Re: acetone and steel/brass corrosion

by MatthewK <MatthewK@[EMAIL PROTECTED] > Jul 5, 2008 at 02:38 PM

On 2008-07-05, BenchMade <gkotr@[EMAIL PROTECTED]
> wrote:

> I saw in a thread earlier- someone saying something about a coating
> (military?) you could apply to protect your blade. What is something
> that you could just wipe on your blade to protect it- and how often
> should you do that- can it be bought in a local store? TIA

I think that was me who said that. It is called mil-spec plus I
think. You could probably buy some at a gunshop. It was
designed to keep gun parts working together properly.

Steve, who's fan club troll here, had good things to say about
it in his enviroment in thailand.

I've never used the stuff so my personal expierence is
limitted. google, and perhaps other posters, is your friend. If
you do get some than please give us a re****t.

matthew
 




 23 Posts in Topic:
acetone and steel/brass corrosion
MatthewK <MatthewK@[EM  2008-07-04 22:35:46 
Re: acetone and steel/brass corrosion
"Lachlan - Grand Exa  2008-07-05 00:10:43 
Re: acetone and steel/brass corrosion
Chilla <charlesanderso  2008-07-05 12:16:51 
Re: acetone and steel/brass corrosion
LarbGai <larbgai@[EMAI  2008-07-04 19:34:16 
Re: acetone and steel/brass corrosion
MatthewK <MatthewK@[EM  2008-07-05 22:31:41 
Re: acetone and steel/brass corrosion
Chilla <charlesanderso  2008-07-06 21:43:25 
Re: acetone and steel/brass corrosion
"steve@[EMAIL PROTEC  2008-07-06 05:02:21 
Re: acetone and steel/brass corrosion
MatthewK <MatthewK@[EM  2008-07-09 20:15:05 
Re: acetone and steel/brass corrosion
Cheesy Bob <cheeseking  2008-07-09 05:41:01 
Re: acetone and steel/brass corrosion
"Michael Koblic"  2008-07-04 21:12:14 
Re: acetone and steel/brass corrosion
nurk_fred2000@[EMAIL PROT  2008-07-04 21:22:52 
Re: acetone and steel/brass corrosion
MatthewK <MatthewK@[EM  2008-07-05 06:15:52 
Re: acetone and steel/brass corrosion
BenchMade <gkotr@[EMAI  2008-07-05 01:34:59 
Re: acetone and steel/brass corrosion
MatthewK <MatthewK@[EM  2008-07-05 14:38:31 
Re: acetone and steel/brass corrosion
Greg Wormald <greg@[EM  2008-07-06 00:30:29 
Re: acetone and steel/brass corrosion
Sean Elkins <sean_elki  2008-07-05 12:36:01 
Re: acetone and steel/brass corrosion
"Michael Koblic"  2008-07-05 14:01:41 
Re: acetone and steel/brass corrosion
BenchMade <gkotr@[EMAI  2008-07-06 01:30:05 
Re: acetone and steel/brass corrosion
BenchMade <gkotr@[EMAI  2008-07-06 01:33:07 
Re: acetone and steel/brass corrosion
"steve@[EMAIL PROTEC  2008-07-06 01:37:13 
Re: acetone and steel/brass corrosion
LarbGai <larbgai@[EMAI  2008-07-06 03:00:40 
Re: acetone and steel/brass corrosion
"Takin & Kanoknu  2008-07-06 18:09:45 
Re: acetone and steel/brass corrosion
Cheesy Bob <cheeseking  2008-07-06 03:32:09 

Post A Reply:
  Go here to Signup

AddThis Feed Button


About - Advertising - Contact - Frequently Asked Questions - Privacy Policy - Terms of Use - Signup

Contact
tan12V112 Mon Sep 8 9:42:20 CDT 2008.